Hi,
I'm Xeros.

each material has specific creep temperature.
So, my client request the creep temperature for Cr-Mo steel and 25Cr-35Ni steel.

I could find web site for provide the creep temperature for material.

However, i think that data on web-site is not enough for reference to client.

Please give me the information about reference book title, code, standard or specification.

Best regards,
 
For Cr-Mo creep data, I would suggest the following publication (it is outdated but very comprehensive in terms of creep data) issued by the ASTM-ASME Joint Committee on Effect of High Temperature on the Properties of Metals or the web site below;

"Report on the Elevated-Temperature Properties of Chromium-Molybdenum Steels" Special Technical Publication No.151

For 25Cr-35Ni steels go here;

Note;
If you would like a printed version of a data sheet, please download and fill in the application form and send it by mail or email as a PDF file. Printed version of data sheet will be sent for free, only to those institutions whose applications have been approved by the Application Review Committee.


postal address: General Affairs S. of Meguro
National Institute for Materials Science
2-2-54 Nakameguro, Meguro-ku, Tokyo 153-0061, JAPAN
Fax. +81-3-3719-2177
email address:
the application form [PDF]
 
Please find below.

- API RP579, Table 4.1
- API STD 530, Annex E
 