Can anyone share some creep data of this material at 700-800 deg F please?

Truly appreciated
 
Replies continue below

Recommended for you

What exactly do you need, stress rupture strength, creep deformation rate? If you have access to ASME Section II, Part D, you can work around creep deformation rate and stress rupture stregnth by using allowable stress values.

The web site below is one of the best I have seen on pressure vessel material creep properties. You can register for free, to access this database;

 
Thanks a lot for the reply, Metengr.

What I need specifically is to estimate the time to get 2-3% creep strain at 700-800 deg F at stess level of 20-30 ksi.
 
You may not find what you are looking for....

A516 Gr. 70 material is carbon steel plate commonly used for tanks and pressure vessels. The ASME boiler code bans usage above ~ 775 F due to a metalurgical degradation known as "graphitization". This type of failure occurs over long periods of time....

This type of degradation is why the more costly alloy steel materials were developed in the first place.


A case study of this failure mechanism is located on:


Why are you interested in this information ?