Dear friends
I work in a Hydropower Construction company for the client. This is my problem.
We have a 90 mtrs *3 chambers surface desilter chamber.So now the struture has an inclined wall near the invert about 1.2 mtrs of ht and running both ways of the chamber.We started pouring M50A20 grade concrete along this patch say 30 mtrs at once since the construction joint is at after every 30 mtrs interval. We have seen cracks along the reinforcement bar cutting the whole width and depth of the concrete.
The crack appears on each shutter(MS shutter plate 1.2*2.5 mtrs. YOu can also view an image to see waht i am talking about.
cement: 480 kg(OPC 43)
water :156 kg
Micro SIlica fume : 38.0 kg (Elkem)
20 mm(crushed) : 560 kg
10 mm(crushed) : 560 kg
crushed sand : 600 kg
Super plasticiser : 3.0 kg(TAM cem)
SLump : initial collapse to 150 mm upto 2 hrs
Slump flow : 480- 550 mm
Possible causes: 1. Autogeneuos shrinkage????
2. Pouring Method: The concrete is poured through a concrete pump. The pipes rests directly on the main rebars. So I assume that the stoke of the pump disturbs the hardening of the concrete. ????
KINDLY HELP ME THIS PROBLEM.
I work in a Hydropower Construction company for the client. This is my problem.
We have a 90 mtrs *3 chambers surface desilter chamber.So now the struture has an inclined wall near the invert about 1.2 mtrs of ht and running both ways of the chamber.We started pouring M50A20 grade concrete along this patch say 30 mtrs at once since the construction joint is at after every 30 mtrs interval. We have seen cracks along the reinforcement bar cutting the whole width and depth of the concrete.
The crack appears on each shutter(MS shutter plate 1.2*2.5 mtrs. YOu can also view an image to see waht i am talking about.
cement: 480 kg(OPC 43)
water :156 kg
Micro SIlica fume : 38.0 kg (Elkem)
20 mm(crushed) : 560 kg
10 mm(crushed) : 560 kg
crushed sand : 600 kg
Super plasticiser : 3.0 kg(TAM cem)
SLump : initial collapse to 150 mm upto 2 hrs
Slump flow : 480- 550 mm
Possible causes: 1. Autogeneuos shrinkage????
2. Pouring Method: The concrete is poured through a concrete pump. The pipes rests directly on the main rebars. So I assume that the stoke of the pump disturbs the hardening of the concrete. ????
KINDLY HELP ME THIS PROBLEM.