Dec 17, 2004 #1 WKTaylor Well-known member Joined Sep 24, 2001 Messages 4,331 Location US Folks... What is/are acceptable welding [wire/rod] alloys for this material??? And per what established [aerospace] practices??? Note: AWS D17.1 does not provide clarity. Regards, Wil Taylor
Folks... What is/are acceptable welding [wire/rod] alloys for this material??? And per what established [aerospace] practices??? Note: AWS D17.1 does not provide clarity. Regards, Wil Taylor
Dec 17, 2004 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Can you provide some current information if you are cracking this material? 1. What filler metal are you using? 2. Current welding parameters? Upvote 0 Downvote
Can you provide some current information if you are cracking this material? 1. What filler metal are you using? 2. Current welding parameters?
Dec 17, 2004 #3 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Wil; Here some background information regarding weldability for this alloy from Carpenter http://cartech.ides.com/datasheet.aspx?i=103&e=156&c=TechArt Upvote 0 Downvote
Wil; Here some background information regarding weldability for this alloy from Carpenter http://cartech.ides.com/datasheet.aspx?i=103&e=156&c=TechArt