We buy parts machined from solenoid quality 430FR (ASTM A 838 alloy type 2) bar. Several parts have cracked completely through from one end to the other right through the center axis of the bar. There is one large flange on the part which the crack does not go completely through the OD. There is no doubt in my mind that the crack is a seam in the bar stock which was present before machining. We are 100% sorting parts at the moment but would like the supplier to check their remaining bar stock inventory.
What sort of non destructive testing is available to find an internal crack in magnetic material like this? The bar stock is approximately 7/8" OD.
We buy parts machined from solenoid quality 430FR (ASTM A 838 alloy type 2) bar. Several parts have cracked completely through from one end to the other right through the center axis of the bar. There is one large flange on the part which the crack does not go completely through the OD. There is no doubt in my mind that the crack is a seam in the bar stock which was present before machining. We are 100% sorting parts at the moment but would like the supplier to check their remaining bar stock inventory.
What sort of non destructive testing is available to find an internal crack in magnetic material like this? The bar stock is approximately 7/8" OD.