Everything seems allright with the above combination but could it be one of the following:
- It was a fillet joint connecting a pig tail elbow (3mm thick) to a lifting lug (8mm thick) with a throat thickness of 3mm - too small?
- The system is a set of headers (4" and 6") hanging on spring supports connected with the above mentioned lifting lug - spring loads weren't considered for the fillet weld size?
Any other thoughts?