Hi All,

Please find the attached the CuSO4 and Zinc Reference Potential Comparison chart for your help to understand that both Reference Electrode potential values are not proportional to each other. Is there a equation to find the conversion as we required to enter the coversion factor to enter into SCADA for remote monitoring purpose.
 
Replies continue below

Recommended for you

Thanks brimmer for a very helpful reply. Further thanks for your reply on my previous question on MAOP issue in our pipe line.

Regards,