Jun 20, 2002 #1 kkc2011 Materials Joined Jun 20, 2002 Messages 1 Location CN Could anyone tell me how to reduce the brittleness for BR. But the percentage of rebound doesn't change.
Could anyone tell me how to reduce the brittleness for BR. But the percentage of rebound doesn't change.
Jun 23, 2002 #2 jklkc Mechanical Joined Jun 23, 2002 Messages 4 Location MY Use Nd (neodymium) BR. Its elastivity is higher and not so brittle. Upvote 0 Downvote
Jun 23, 2002 #3 jklkc Mechanical Joined Jun 23, 2002 Messages 4 Location MY Did you used Li (Lithium)-BR? It is the most brittle among BR Upvote 0 Downvote