It was our experience that Stellite #6 was totally unsatisfactory for use in 55%-65% bleached and unbleached high purity HNO3 at any temperature. It was also unsatisfactory in 20% HNO3 at 100?C.
Once you added organics, especially the acids, the dissolution is straight forward in a hurry.