Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations JAE on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Corrosion resistant stacked metal coatings on mild steel for HCl and NaCl /seawater

Status
Not open for further replies.

thickfilm1

Materials
Joined
Apr 12, 2012
Messages
5
Location
US

We are testing metal coatings applied to mild steel for marine petroleum well oil tool applications.
We are having some success in seawater using Al-magnesium base with certain Hastelloy
mid stack and chromium top layer , all in specific proportions .
They are applied using our patented ion plating process and are very thin ( < 25K Ang. ) .
The goal is to protect mild steel against sea water , < 5% HCl and H2S in petroleum wells .
Any suggestions for a metal that will maintain NaCl resistance and also protect against HCl with our current stack of Al/magnesium, Hastelloy , chromium ?

We know we can use Pd/Ag but it seems to reduce salt ( NaCl ) resistance .

Some alloys can be evaporated and still maintain some properties but it is surprising which ones work and don't .
Any help is appreciated.
 