Nov 8, 2008 #1 sunshine419 Materials Joined Aug 7, 2008 Messages 32 Location GB Please i will like to know the corrosion rate of copper in vinegar in terms of depth of material loss per year(mmpy).
Please i will like to know the corrosion rate of copper in vinegar in terms of depth of material loss per year(mmpy).
Nov 9, 2008 #2 strider6 Materials Joined May 4, 2007 Messages 616 Location IT vinegar contains acetic acids in concentrations, usually, of 4-10%. from the data that i've found the corrosion rate for Copper for conc above 5% is >50 mpy. hope this help S Corrosion Prevention & Corrosion Control Upvote 0 Downvote
vinegar contains acetic acids in concentrations, usually, of 4-10%. from the data that i've found the corrosion rate for Copper for conc above 5% is >50 mpy. hope this help S Corrosion Prevention & Corrosion Control