Dear All,

I'm developing a solar water heater which combines the collector and storage tank together, heating portable water directly. The product has been made, and tested. The problem we found after 6 months testing is pitting/crevice corrosion on the top of SS 304 tube (welding area).

My case is:
- SS 304 long tube welded on the bottom and top
- portable water in the SS tube, regular working temp. 35-210F.
- Pressure <90 psi
- Max temp. 600F when the SS tube is empty and baked under the sun.

There is very little corrosion found at the bottom or in the middle of tube. Pitting/crevice corrosion is only found at the top around welding area. The solar hot water was rarely used when testing. I suspect that the pressured steam with chlorine in portable water is causing the corrosion, and the S.S. material structure was damaged at the welding area.

My question is:
-Any coating material can be applied at the top of welding area inside the S.S. 304 tube? but it can not contaminate the portable water under high temp. and pressure.
-Any welding process or procedure can be used without destroy S.S. 304 material structure in this case?

Thank you very much for your help and advice!

Dixie Solar
 
Thank you very much! Ed, you are very helpful!
 