Due to an error in wall thickness calculations we have two pipelines connected together with a difference of 16mm. this crates an 8mm raised lip on one side.
The fluid is a warm brine produced water highly corrosive fluid with a reasonable amount of dissolved iron, the system is designed to avoid ingrss of oxygen.

My question is: will this lip create turbulance and/or induce a bacterial growth area and hence become a corrosion mechanism.
 
It depends on flow conditions. What is the design process stream velocity thru this pipe?
 
It could become a site of enhanced corrosion (rather than a 'mechanism'). Can you not match bore a little bit to give a transition?

Steve Jones
Materials & Corrosion Engineer
 
The rating of the system is 1500 ILB

I may the contractor ask to chamfer the flanges to help the transition
 
From a strength perspective, I doubt very much that the flange will be the weak link. You can probably taper the edge of the one flange quite a bit, with the limiting factor being cost.

As others have stated - reducing turbulance will only help.
 