Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations LittleInch on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Corrosion Information

Status
Not open for further replies.

Chpal1984

Mechanical
Joined
Nov 19, 2014
Messages
31
Location
GB
Hi,

I was wondering if anyone on here can help me. I'm looking for corrosion data for Alloy 718, AM 350, Alloy 42 and 316 SS, when exposed to different fluids (e.g. Acetic acid, Acetyl Chloride, Acetone etc). I've tried my trusty NACE Corrosion Survey Database, but these metals aren't in it. Does anyone have any suggestions as to where I might find the data?

many thanks
 
They are different animals.
Alloy 42, if you are meaning Fe-42Ni, it is not even considered to be corrosion resistant. it will rust at humid environments even at room tempreature.
718 is a superally (high temp alloy)
Am350 is precipitate hardenable, general corrosion resistance is similar to 316
316 cannot be hardened by heat treatment.
 
Or the Compass corrosion guide.
Concentration, impurities, and temperature will be critical.
Though some of these, such as acetone will not effect any of these metals.

= = = = = = = = = = = = = = = = = = = =