trainguy;
yes. Generally speaking, corrosion fatigue in most metals can be characterized by crack propagation that is typically transgranular (thru grains) with minimal, if any, primary crack branching. You could possibly see corrosion products along the primary crack surface and near the crack tip.
SCC on the other hand typically exhibits noticeable crack branching with a crack path that can be either transgranular or intergranular (along grain boundaries).