I have a automatic transmission control application with sliding aluminum spool valves running in a aluminum valve body. I am having difficulty with controlling the corner break in the spool valve, after the Hard coat anodizing process. The uneven corner profile creates a space for debris to collect and produces a sticky valve.
Are there any solutions?
Is this the right forum for this discussion?
Are there any solutions?
Is this the right forum for this discussion?