Aug 12, 2016 #1 nawlins Computer Joined Sep 14, 2005 Messages 8 Location US what alloy contains 64% Ni and 30% Cu thanks
Aug 12, 2016 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Where is the other 6% for a mass of 100%? This could be Monel. Upvote 0 Downvote
Aug 12, 2016 #3 EdStainless Materials Joined May 20, 2004 Messages 16,366 Location Waukesha WI USA Must be a variation of Monel 400. 63-70% Ni, up to 5% Fe+Si+Mn (they each have limits), bal Cu = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, Plymouth Tube Upvote 0 Downvote
Must be a variation of Monel 400. 63-70% Ni, up to 5% Fe+Si+Mn (they each have limits), bal Cu = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, Plymouth Tube