I am looking for recommendations on bonding copper foil into a fiberglass or carbon fiber laminate. The copper foil will be near the surface of the laminate but will not be exposed to corrosion environments.
I am having a hard time getting a good bond. Would the use of BR127 or BR6747 help me alot? I do not want to grit blast the copper foil if possible. I do want a pretty good bond though because of the CTE mismatch and a service temp going from -40 F up to 160 F.
Suggestions are greatly appreciated.
I am having a hard time getting a good bond. Would the use of BR127 or BR6747 help me alot? I do not want to grit blast the copper foil if possible. I do want a pretty good bond though because of the CTE mismatch and a service temp going from -40 F up to 160 F.