Hi,

I am fairly familiar with the use of anodizing/alodining aluminum surfaces to prevent corrosion, but are there similar processes for copper? I have 110-alloy electrical grade copper shims which I would like to treat, and the coating should be RoHS-compliant. Thanks in advance.
 
The only protective coating we used with Cu was Ni with copper gaskets and Ag with electrical components.
 
What environment? Cu is passive for many environments.

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
The copper shims are to be placed between MDR connectors and an alodined aluminum back plate inside a camera. EMI shielding is a requirement, so we are trying to prevent any loss of conductivity in the copper. As far as I'm aware, the camera is to be used in normal ambient indoor conditions.
 
Silver over Cu is quite common on electrical connections like the buss bars in substations. The conductivity actually will increase under certain conditions.

There a kits available from my electrical supply houses that can do small silver plating jobs for testing.
 