copper corrosion in HF

Status
Not open for further replies.

wildRover

Materials
Oct 3, 2003
4
Usually copper is reported as resistant to HF corrosion in air free enviroments, but if I attack it with HF-water vapor can I attack it? And if it is the case, how does the reaction rate changes with temperature and HF concentration?
 