I have read in many suppliers sites/catalogues about the role copper plays in aluminum electrical equipment. Most of the time, manufacturers take great pride in identifying that they have no more than 0.1%, 0.4% or 1.5% copper in their aluminum products (typically cast, not forged). Can you please advise what % is the best in so far as application in a marine (salt spray) environment is concerned? I am sure that someone did a study at one point and identified that for increasing copper content in a marine environment, more pitting occurred as a result of increasing copper. Do you know where I may find the results of such a study? Finally, how does one ensure low copper content? Is it separated during casting or before that?

Thanks

Ken Almon
 
Replies continue below

Recommended for you

The Metals Handbook states that any copper above "a few tenths of a percent" causes the problem which is a dissolution and redeposition of copper causing galvanic couples. 3003 with 0.2% max or 5xxx grades with 0.1% max ought to be fine, or as good as you'll get if you have to use aluminum.
 