Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Cooling lubricant/emulsion treatment for the metal processing industry

Status
Not open for further replies.

macabihaifa

Chemical
Nov 28, 2003
12
Hello,

In oeder to improve economics and enviromental aspects of a/m subject,

does a continuous treatment exists so there is no down time of the metal processing machine?

What are the main features of such a system? a process flow diagram or block diagram can be helpful.

Regards,
M.
 
Replies continue below

Recommended for you

Is this coolant for cutting operations?
I have seen many centralized systems, all machines drain back to one tank.
This tank will have excess capacity and provide a buffer for the system.
There the fluid has oil separated, it is filtered (settling, screen, coarse filter, fine filter), and it is cooled.
In some cases I have seen that a small flow is bled off and it is made up with fresh addition.
In other cases they drain some fraction (10-25% depending on application) of the system each week and make it up with fresh fluid.
At the minimum the concentration needs to be monitored so that the mix can be kept correct.
I have seen this with mills, lathes, saws, hones, cold drawing.
You can combine whatever machines are using the same fluid.

= = = = = = = = = = = = = = = = = = = =