Convergence issue in an indentation model with Drucker-Prager plasticity

Status
Not open for further replies.

quentinflm

Materials
Joined
Nov 5, 2015
Messages
2
Location
ES
Hi all,

I recently started to use Abaqus in order to simulate the spherical indentation of a porous layer.
Here is a quick description of my model (Download here the related files).
2D axisymmetric model with 2 parts:
- the indenter: discrete rigid body, real shape of the indenter defined by a spline curve (so it's not exactly an arc of circle)
- the sample with 2 sections:
=> the porous coating: elastic material with Drucker Prager Plasticity
=> the bulk: elastic material
Elements: CAX8 and CAX8-R.
Interaction: hard contact, no friction
Step 1: displacement control (loading and unloading)

I have the following convergence issues:
- If the coating is considered as elastic (no plasticity), I manage to get convergence. However I noticed 2 strange things that I dont't understand:
=> If I reduce the increment size from 0.1 to 0.01 I lose the convergence beyond a certain displacement
=> If I use a finer mesh under the contact, I lose the convergence beyond a certain displacement

- When I try to use the Drucker Prager plasticity, I cannot get convergence beyond a certain displacement

I’m a bit lost… I don’t know where the problem(s) come from. Is it contact related ? mesh related ? geometry related ?

I would be very grateful if you could suggest a methodology to solve this.

To finish one basic general question: how to know what caused the divergence in a simulation ? Sometimes I don’t have any warning before it stops and it is not clear either in the Message file.

Thank you very much for your help
 
Have you tried the unsymmetric equation solver?


The reason for convergence issues can be found in the .msg file. See Getting Started 8.4 Example: nonlinear skew plate
 
Thanks for your reply. Yes I am using the unsymmetric equation solver. Thanks also for the reference, I will check it.

However in the message file, the last increment finishes with

THE CONTACT CONSTRAINTS HAVE CONVERGED.
[...]
THE FORCE EQUILIBRIUM EQUATIONS HAVE CONVERGED
[...]
THE MOMENT EQUILIBRIUM EQUATIONS HAVE CONVERGED"

I don't see any error here, that's why I was asking
 