Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations KootK on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

conver rate 2

Status
Not open for further replies.

xiangxi

Civil/Environmental
Oct 30, 2002
6
Hello all,

Does anyone know how to convert Agg Base or AC surface from cubic yard to ton? Can you be kind enough to provide the source of information? I appreciate it.

Xiangxi
 
Replies continue below

Recommended for you

What kind of aggregate base are you referring to?

Hot mix usually weighs 2 tons/cyd or thereabout, depending on the aggregate used.
 
Thank you for your response. It's a Type II aggregate base. Do you have any clue where this number come from and how?
Xiangxi
 
The following conversion factors for base course and blacktop paving where given to me by a paving contractor as the ones he used for estimating:

Material Compacted Tons/SY Tons/CY
Thickness

Stone Base 6" 0.33 1.98
8" 0.44
10" 0.58
12" 0.66

Blacktop 1" .055 2.25
2" .110
3" .165
4" .220

However, you can compute any of these yourself using the unit weight of the material, which can be found in any engineering ref. book or AISC manual:

tons/cy = [(lbs/cf)x(27 cf/cy)]/2000 lbs/ton

Hope this helps!
 
Thank you very much. It's really helpful.