What are the most common materials used? How important are Ag-In-Cd alloys in control rods? Have they been superceded by other materials in newer designs?
 
Replies continue below

Recommended for you

In my experience with BWRs, boron carbide (b4c) powder in tubes; once the boron absorbs a neutron, it is "used up"; newer designs use hafnium, because after absorbing neutrons, it becomes other isotopes of hafnium that are also good neutron absorbers.
 