sistersparky
Electrical
Hi, I know a similar question was raised further down the list but the thread has been closed, so here we go...
I am restoring a 70's beast & I'm wondering about using a 95% zinc spray ("cold galvanizing") to shoot INSIDE frame members (where I can't possibly prime & paint effectively -- or does someone REALLY have solutions for everything? ;D)
The spray is relatively cheap, $10 a pop. I figure it's worth a try, but the previous thread raised some questions in my head.
My understanding of sacrificial anodes (though my chemistry is admittedly rusty) was that it would protect a fair amount of surrounding metal as well... not JUST the touching parts. Just how localized is the protection offered, and will I really just be concentrating a rust attack in areas I can't spray at all?
I am restoring a 70's beast & I'm wondering about using a 95% zinc spray ("cold galvanizing") to shoot INSIDE frame members (where I can't possibly prime & paint effectively -- or does someone REALLY have solutions for everything? ;D)
The spray is relatively cheap, $10 a pop. I figure it's worth a try, but the previous thread raised some questions in my head.
My understanding of sacrificial anodes (though my chemistry is admittedly rusty) was that it would protect a fair amount of surrounding metal as well... not JUST the touching parts. Just how localized is the protection offered, and will I really just be concentrating a rust attack in areas I can't spray at all?