Oct 15, 2002 #1 STEVEBR Mechanical Joined May 7, 2002 Messages 12 Location GB WHERE CAN I FIND INFORMATION RELATING TO THE COPPER ALUMINIUM CONSTITUTIONAL DIAGRAM
Oct 15, 2002 #2 TVP Materials Joined Apr 12, 2002 Messages 4,592 Location US ASM HANDBOOK Volume 3 Alloy Phase Diagrams is one place to start. You can obtain this book from ASM International at http://www.asminternational.org. Upvote 0 Downvote
ASM HANDBOOK Volume 3 Alloy Phase Diagrams is one place to start. You can obtain this book from ASM International at http://www.asminternational.org.