Hi, I am a frustrated engineer dealing with a plastic injection moulder. This company is providing an electrical connector to us. During several months the main quality concern is the height of the female connector opening (internal feature) being warped in the that our operators have troubles to fit the male connector in there since the opening is being reduced to be lower than the min limit. The vendor says that they need an extra dimension in the middle in order to justify an extra measurement in their process. According to rule #1 the size limits apply to the whole extent of the feature, so there is no need for other specification. Could someone comment on this, please? I already started to hesitate if I am correct to demand that dimension to be corrected either by process or mold size fixes, or just must give up and sort the incoming inventory with a block gage.