What is the best material for lining a concrete tank receiving Ultra Filtrated Secondary Effluent and directly feeding Reverse Osmosis System (no cartridge filter between the tank and the RO system)? CIM, and Fiber Glass has failed.
Thanks
 
When you say the lining has failed, what has failed it? Was it chemical attack? What was the mode of failure? Concrete is pretty tough under most all exposures, except acids.
 