Apr 15, 2013 #1 Gillespie Structural Joined Aug 3, 2009 Messages 26 Location US For a 6" thick concrete slab on grade (which will have radiant coils) I am using wire mesh (2" from the top) then an layer of #4 bars at 16"o.c. each way. Recommending saw cuts after. Any recommendations to reduce further cracking........
For a 6" thick concrete slab on grade (which will have radiant coils) I am using wire mesh (2" from the top) then an layer of #4 bars at 16"o.c. each way. Recommending saw cuts after. Any recommendations to reduce further cracking........
Apr 15, 2013 #2 BAretired Structural Joined Nov 16, 2008 Messages 11,044 Location CA Where do the guys stand while placing the concrete? BA Upvote 0 Downvote