An owner has indicated that he is not happy with the appearance of a concrete floor (the floor is meant to be exposed). The floor has a cloudy/splotchy appearance. Any thoughts on what may have caused this? Perhaps a curing issue? I have attached a photo, and will add more following this post...
 
 http://files.engineering.com/getfile.aspx?folder=edc29299-aa5c-46d0-9853-685869e62f0e&file=IMG_1811.jpg
Replies continue below

Recommended for you

The cause of that is that it's concrete. ;) The surface looks to be a hard-steel-trowel finish to a near shine, which can lead to varied coloration in the surface.

In my opinion, short of a well documented mock-up procedure, what you see is what you get. Though the sawcut control joint edges are a little rough, I'd be pleased that there are no cracks.

To Burnish or Not to Burnish your Concrete?

NRMCA CIP 23 - Discoloration
 
I agree - just looks like concrete to me.

There's clearly a lot in this though
What did the owner expect? Marble?
Just google image polished concrete and you'll see many that look just like this.

Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
 
I agree that there are noticeable patterns in the finish, but I would not deem it unacceptable (unless there were provisions for a particular finish or appearance). It seems like most of the variation occurs at or near slab joints. If it occurs at a construction joint, it may be that the finishing operations were done too late or too long. The slab edges usually set earlier than the middle areas of a slab. Steel trowel may have gone over the slab edges after their initial set.
 
This is typically caused by too much bleed water bringing fines to the surface and then hard troweling the surface. This can cause a longer term durability issue. Consider taking a core in an inconspicuous place and having a petrographic examination of the core.

If you don't want to go through that process, I would suggest a light acid wash using citric acid, followed with the application of a surface hardener such as Prosoco Consolideck or other silicate hardeners.
 