peconsultant
Structural
I am trying to put together an estimate for a concrete repair project. The project consists of injecting concrete columns with an epoxy resin. RS Means shows a production rate of 80 lf per day. I need to estimate what percentage of the labor is spent on prepping the concrete, injecting the concrete, and cleaning the concrete. Does anyone have any insight on this. My contractor has been useless in trying to put together this information.