Hello everyone,

I have modeled compression test on concrete cube in Abaqus/Explicit. For concrete I have used Concrete damaged plasticity model. I have assigned displacement as BC (Smooth amplitude) in Reference Point at the top of the cube, and I have coupled RP with the top of the cube. For concrete cube I have used C3D8R elements.

For history output I have requested Reaction force in RP and energies for whole model.

But job won't finish. I get an error:

The part map file "D:\Marko\Concrete\Compression.prt" is corrupt, does not exist, or cannot be opened.

The elements contained in element set ErrElemExcessDistortion-Step1 have distorted excessively.

I am sending you pictures of Reaction Force and PE and PEEQ of Cube (results until job cancelation).

Can anyone tell me why and give me some suggestions?
 
 http://files.engineering.com/getfile.aspx?folder=f0754a49-87de-40fb-81ed-d1b6630157a0&file=Concrete_cube_a.png
Replies continue below

Recommended for you

Status
Not open for further replies.

Part and Inventory Search

Sponsor