I have a couple of centrifugal gas compressor units which have gone out of balance at the same time - this has coincided with problems with a system that injected wax inhibitor into the gas stream, so it looks as if waxy deposits on the rotors are responsible.
I have tried a wash to eliminate salt deposits (with the compressor at rest, injecting water into the bottom of the barrel and turning the rotor by hand through several 90 degree intervals) without improving the situation, so I now want to try a wash using a hydrocarbon solvent.
I have 3 constraints:
a) The wash fluid should not be dangerous to personnel - e.g. no benzene
b)There is a slight chance that the wash fluid will enter the dry gas seals, so the solvent must not dissolve viton O-rings
c)Since these units are located offshore there are environmental requirements - just in case any of the wash fluid escapes into the sea, it must be reasonably doplhin friendly
I have contacted several major chemical suppliers, but the quanitities that I am looking for (intially 200 litres) haven't don't seem to generate much interest.
Anyone able to recommend a wash fluid that might help?
thanks
I have tried a wash to eliminate salt deposits (with the compressor at rest, injecting water into the bottom of the barrel and turning the rotor by hand through several 90 degree intervals) without improving the situation, so I now want to try a wash using a hydrocarbon solvent.
I have 3 constraints:
a) The wash fluid should not be dangerous to personnel - e.g. no benzene
b)There is a slight chance that the wash fluid will enter the dry gas seals, so the solvent must not dissolve viton O-rings
c)Since these units are located offshore there are environmental requirements - just in case any of the wash fluid escapes into the sea, it must be reasonably doplhin friendly

I have contacted several major chemical suppliers, but the quanitities that I am looking for (intially 200 litres) haven't don't seem to generate much interest.
Anyone able to recommend a wash fluid that might help?
thanks