I have some conflicting information on this. One source gives 170 GPa tension and 146 GPa compression, another almost reverses this: 152 GPa tensile vs. 164.5 GPa compessive! This is standard sort of 12k tows 100% 0 degree tape 60% Vf in ordinary prepreg epoxy.
Does anyone know which way around it "should" be? (I suppose it's just possible both are right and it can vary.)