Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations JAE on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Compatibility of Spiral Wound Gasket (SPW) with Flanges having Different Surface Finish

Status
Not open for further replies.

Awais Arshad

Mechanical
Joined
Oct 27, 2022
Messages
7
Location
PK
Hi all,

We have a case where the mating flange has different surface finish compared to the top flange; one flange has a surface finish value of Ra 3.2-6.3 um, while the other has a surface finish value of 1.6 um.

As per my literature research, the SPW gasket works find under such configuration. Still, being a forum of expert engineers, will appreciate if the members can shed light on the case i.e. if a Spiral Wound Gasket will operate or work fine @ DP = 35 kg/cm2g & DT= 220 dC under different flange surface finishes as mentioned earlier.

Regards,
Awais
 
The only times I have had problems with spiral gaskets sealing the problem was either bad alignment of the flanges or insufficient clamping force. The surface finish is recommended to have roughness in a phonograph pattern, but is otherwise less critical to sealing.
Recommendation is to follow the guidance in the OEM technical manual (see the flexitalic design manual).
If you encounter a situation where the spiral component of the gasket unwinds, consider ordering the gasket with an inner ring.
 