Hello Guy,
maybe this helps you:
structuralengineer
Issue 22-2000 (21 Nov 2000)
Limits on load carrying capacity of flat slabs
Synopsis
Design of flat slabs is usually based on separate considerations of flexure and shear, with empirical rules similar to those used in design of beams and continuous
slabs. Additionally, shear capacity of a flat slab has to account for its distinctive mode of failure known as ‘punching failure’ or breaking away of a portion
surrounding the column from the rest of the slab. Provision against such failure is often the critical design requirement for flat slabs with or without openings
adjacent to the columns. While links are normally provided to enhance the punching shear capacity, the current Codes of Practice stipulate limits on the loadcarrying
capacity of flat slabs. Such limits govern the thickness of the slab and, therefore, have a direct influence on economy of construction. This paper examines the limits
on loadcarrying capacity of flat slabs supported on internal and rectangular columns, which are given in BS 8110 and Eurocode EC 2, with the help of tests on slab
specimens with and without openings.
S. B. Desai, OBE, BE, PhD, CEng, FIStructE formerly, DETR
Keywords: flat slabs, design, BS 8110, Eurocode 2, comparing, shear, load tests, research