Please let me know which is the commercial name for polyethylene terephthalate? Which is the basic chemical reaction to produce PET?
Aug 14, 2001 #2 pittguy727 Chemical Joined Jul 31, 2001 Messages 10 Location US There are alot of trade names for PET... one company we bought off of before is eastman. http://www.eastman.com I think they are merging or becoming veridian?? But you can contact them for information on PET's Upvote 0 Downvote
There are alot of trade names for PET... one company we bought off of before is eastman. http://www.eastman.com I think they are merging or becoming veridian?? But you can contact them for information on PET's
Aug 21, 2001 1 #3 phoward Chemical Joined Aug 17, 2001 Messages 54 Location US Mylar (Dupont), Dacron, Skotch-Pak (3M) and Tinuvin are some related names with different grades. Check out http://yarchive.net/chem/pet.html. Do a search on Goggle and you will get lots of names. Upvote 0 Downvote
Mylar (Dupont), Dacron, Skotch-Pak (3M) and Tinuvin are some related names with different grades. Check out http://yarchive.net/chem/pet.html. Do a search on Goggle and you will get lots of names.