Is there anyone who could advice on :

By Spraying Cold Galvanizing Compound Zinc Rich Coating on pocket Kit(Material : A350LF2), will there be any chemical reaction?

After spraying with this cold galvanizing compound,will the pocket kit(Material : A350LF2) be rust resistance in a salty environment? (e.g. Beside the Sea)

The galvanizing compound contains:-

1) Zinc Dust C.A.S. 7440-66-6,
2) Toluene C.A.S. 108-88-3,
3) Propane C.A.S. 74-98-6,
4) Isobutane C.A.S 75-28-5
5) NAPTHA C.A.S. 8030-30-6

Look forward to anybody's kind advice.

Thanks,
ndnck


 
The spray will not result in a chemical reaction with the steel being sprayed. I don't see how there is any bonding to the object, but I trust that it will stick on the steel.
If there is a bond to the steel, the steel will not rust until the zinc has been consumed by corrosion, at which time the sacrificial anode, i.e. the zinc particles, no longer will protect the steel and rust will commence.
 