We are trying to model a roadway FEM in PLAXIS. Where could I find values for the Cohesion of asphalt or related wearing surfaces?
 
Replies continue below

Recommended for you

The first place that I would look for this information is with the suppliers of asphaltic cement, emulsified asphalts, admixtures, etc. Colas Group for example maintains a large research and development department.

If you are looking for a general range of typical values, try the Turner Fairbank Highway Reasearch Center (FHWA) or the Asphalt Institute.

What exactly are you modeling?
 
Thanks. I'll take a look.

We are creating a FEM of a Concrete Culvert. It's for a Level 1 Load Rating for NY DOT.

 