Code Case 2235 Weld Procedure - Impact Testing HAZ's 1

Status
Not open for further replies.

weldtek

Materials
Feb 12, 2005
897
As many are likely aware the requirement for impact testing HAZ's in thicker materials changed with the 2013 Ed. UG 84 (g)(2)
Some of you may have seen Code Case 2235 but if not it may be helpful to know that it allows for the use of PQR's qualified by the old rules ( prior to 2013) thru 2017. Our AI provided this info to me and I thought I'd share it.
 