The company that I work is trying to cocure decorative laminates (thermoplastic cover sheets) onto our thermoset prepreg parts. We would thermoform the laminate first then place it in the mould. Does anyone know if this is feasible and where I can get further information on this subject? The Decorative Laminate companies all suggest I apply the coverings with an adhesive after curing the prepreg.
 