hi,I am designing a pipeline and I have below conditoions:
I have to use steel pipe in a place that is in cement and also the water that is to transfer is salty.
I want to know if there is any standard for coating and lining protectives for the ebove condition.
Thnx
 
Replies continue below

Recommended for you

Why do you 'have' to use steel pipe? Steel and salt don't mix. Changing from one pipe material to another may also give you problems. What pressures are you running?
 
Check the possibility of using SIGMALine 2000 produced by Sigma Coatings.
 
Try giving us dimensions, design and operating conditions, and your reasons for believing that the water is corrosive. We will try to take it further thereafter.

Steve Jones
Materials & Corrosion Engineer
 