Hello
I simulated a interaction between an air layer (12 cm) and a concrete plate (12 cm). My doubt is:
1) The temperature gradient between the top face and the bottom face, of the air layer, shouldn't be smaller, after 75 minutes? (see Annex 1). I am finding a difference of 900 degrees.
I think, after a time, this air layer should have the same temperature, in top and the bottom faces. I expect to see it.
Boundary condition utilized in Air Layer:
- Inlet: Temperature = Furnace (see Amplitude)
- Outlet: Pressure = 0
- Co-simulation = Interface between air layer and concrete plate
Abaqus File (Plate.CAE): Link
Abaqus File (Plate.JNL): Link
Problem:
Annex 1 - AIR LAYER results:
I simulated a interaction between an air layer (12 cm) and a concrete plate (12 cm). My doubt is:
1) The temperature gradient between the top face and the bottom face, of the air layer, shouldn't be smaller, after 75 minutes? (see Annex 1). I am finding a difference of 900 degrees.
I think, after a time, this air layer should have the same temperature, in top and the bottom faces. I expect to see it.
Boundary condition utilized in Air Layer:
- Inlet: Temperature = Furnace (see Amplitude)
- Outlet: Pressure = 0
- Co-simulation = Interface between air layer and concrete plate
Abaqus File (Plate.CAE): Link
Abaqus File (Plate.JNL): Link
Problem:

Annex 1 - AIR LAYER results: