We supply Cr-Si springs for a spring loaded clutch disc for class 8 trucks. The spring life was not satisfactory, but we fixed that by nitriding them. Now, the customer has a perception that iron oxide fretting residue is a concern and is looking for solutions (to a non problem IMHO). Fretting occurs between the springs and the pockets in the clutch disc as well as the driven and non driven discs. Ideas I have come up with include TiN of the steel disc, dry film lube on the springs and/or steel discs, laser hardening of the spring pockets, slurry deburr of the spring pockets. Anybody got any other ideas for surface treatments?
 
On several occasions I've used bronze, either applied by brazing or a disk brazed to the socket material at the bottom/face of the socket to alleviate wear and recovery of worn spring sockets.
I have also used bronze to recover some very worn clutch housings were the OEM parts were steel plate on steel housing.

 