Hello -
We are cladding C276 to HY 80 and it seems that a common practice is to ensure that that the iron levels, in the welds, are below 10%. Does anyone have a reference for this rule? Any texts that mention this threshold?
Any help would be appreciated.
thanks,
Erik
We are cladding C276 to HY 80 and it seems that a common practice is to ensure that that the iron levels, in the welds, are below 10%. Does anyone have a reference for this rule? Any texts that mention this threshold?
Any help would be appreciated.
thanks,
Erik