Chrome carbide diffusion?

Status
Not open for further replies.

nawlins

Computer
Sep 14, 2005
8
Why would a piece of 3166ss have a 26% chrome content after it has corroded? Is this what is known as chrome carbide diffusion.
 
Replies continue below

Recommended for you

Well, it depends what you mean by "have a 26% Chromium content". It could be that you are analysing what is left over after severe corrosion, which is likely to be regions of higher Chromium content. It could also be your analysis technique, or it could be that you have sampled a spot of sigma phase or similar.
 
All of the areas like that read the high chrome content. These areas are also a dark red like a dark colored rust but it is in tact and hardness values are in the 600 vickers areas.
 
Are you sure the material is 316 SS? This level of hardness is inconsistent with 316SS. Was it nitrided?
 