It isn't the oxidizer part that attacks systems, it is residual acids in the solution from the production of CD.
When CD is produced as a gas on demand the salts (that dissociate as acids) stay in the reactor and the CD gas is very near non-corrosive.
= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube