Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations JStephen on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

CHILLED WATER COPPER PIPE FITTINGS

Status
Not open for further replies.

schola

Mechanical
Joined
Apr 13, 2005
Messages
38
Location
VE
Dear sirs,

I am specifiacting M Hard Copper Tubing for chilled water system. My question deals with choicing of fittings. What do you think is the most advaisable:

Cast brass?
wrought copper?
wrought brass?

Soldered, threaded?

Working pressure will be 90#.

Thanks in advance.

schola
 
There is no practical way to thread Type M copper. It's too thin. Soft solder wrought copper fittings.
 
Wrot copper fittings, pressure pattern, type M pipe, either 95/5 solder or silver solder if it is installed in inaccessible finished locations.

If you want threaded fittings, valves and etc so piping may be disassembled for maintenance, use swet to thread couplings.
 
Have you given some thought to plastic such as CPVC
CPVC piping is suitable for hot and cold water distribution has a 400 psi pressure rating at room temperature, and a 100 psi pressure rating at 180 F. Schedule 80 can be welded or threaded.
 
We use PVC down here, its year round cooling. Does black iron cost more than copper these days?

Must be small mains to be running type M copper

Take the "V" out of HVAC and you are left with a HAC(k) job.
 