What are the factors controlling the selection of using oil or water soluble corrosion inhibitors for trunk lines.

Thanks every body

Abdulla
 
Replies continue below

Recommended for you

Would not it depend upon what fluid is being pumped or sitting static in said trunk lines?
If oil-based, I suspect you would want oil soluble corrosion inhibitor, as water may be forbidden in the line.
 